Specifications:
- Working temperature: 1350 Celsius
- Main chemical composition:
- Al2O3: 60 ~ 65
- SiO2: <20
- Fe2O3: 0.2 ~ 0.3
- Delivery condition: Liquid and looseness
- Packing form: Liquid packing in pail, looseness packing in sack.
- Conserving time: Three months
- Using explanation: After mixing liquid and looseness it has been reacted for 5 ~ 12 hours.
- Notice: After constructing, it may dry by fire when the process of air-dry makes slowly.
Features:
- High temperature coating: coating mainly use of sctawling on the surface of refractory fiber lining for raising worling temperature of furnace lining and wind erosion resistance of furnace lining.
Ordering information:
- Minimum Order: Negotiable set