Sri Lanka Rubber Manufacturing & Export Corporation Ltd.

Send an inquiry
Standard Lanka Rubber (SLR L)

Product ID: P02-2

Standard Lanka Rubber (SLR L)

Manufactured using filed rubber latex and according to the international specifications. Identical in all respects to SMR L.

Specifications:
  • Dirt (retained on 44 micron mesh) %wt: 0.021
  • Ash % wt: 0.18
  • Volatile matter % wt: 0.28
  • Nitrogen % wt: 0.33
  • Initial Wallace Plasticity (Po): 45.0
  • PRI (Pao/Po) x 100: 78.0
  • Lovibond Color Index: 1.5
Features:
  • F/P: Food and pharmaceutical grade
  • SP: Superior Processed
  • H/M: High Money Viscosity
  • L/N: Low Nitrogen
  • Y: Yellow Fraction


No. # SLR F/P SLR SP10 SLR H/M SLR L SLR L/N SLR Skim Grade SLR Y
% Dirt(Max) 0.02 - 0.03 0.03 0.5 0.10 0.10
% VM(Max) 0.6 0.6 0.6 0.6 0.6 0.6 0.6
% Ash(Max) 0.5 0.75 0.3 0.5 0.1 0.1 0.75
% Nitrogen 0.5 Max - 0.5 Max 0.5 Max 0.1 Max 0.6 Min 0.6 Max
P0 (Min) 30.0 40.0 30.0 30.0 30.0 40.0 30.0
PRI (Min) 60.0 60.0 60.0 60.0 60.0 60.0 50.0
Color low bond Grayish Brown No. # No. # No. # Gray Brown Yellowish Brown
Units No. # 3.0 3.0 3.9 No. 3 No. # No. #
Relax Modulus (NR 100) - - 6.5 6.0 6.0 8.5 8.0
Acetone Extract(Max) % 3.0 - 3.0 3.5 3.5 - 8.0
% Rebound Resilience(min) - - - - 80.0 - -
Level of Residual Toxins No1 - No 1 - - - -
Soluble Protein Content (Max) 0.05 - - - - - -

Main Products:
centrifuged latex, pale crepe rubber and foam mattresses

Send an inquiry